Skip to main content

Journal for Biophysical Chemistry

Table 2 Fabrication times and resultant dimensions for two different strategies to fabricate melt electrospun tubes

From: Design and Fabrication of Tubular Scaffolds via Direct Writing in a Melt Electrospinning Mode

Case

Fabrication time (min)

Effective resultant vector speed (mm/min)

Weight (mg)

Average fiber diameter (μm)

1a

22

735

15.2 ± 3.3

25.7 ± 1.8

1b

22

901

14.8 ± 2.5

22.4 ± 1.8

1c

22

1,274

15.7 ± 2.9

19.9 ± 0.9

2a

13

1,273

11.1 ± 1.2

20.4 ± 1.8

2b

22

901

17.5 ± 0.7

26.3 ± 3.2

2c

38

735

37.4 ± 1.3

27.7 ± 2.4