From: Surface anchored metal-organic frameworks as stimulus responsive antifouling coatings

Figure 2

Viability and adhesion analysis of C. marina in contact with Cu-SURMOF 2. Fluorescence microscopy images of adherent bacteria after BacLightTM bacterial viability staining on (A) MHDA SAM and (B) Cu-SURMOF 2 (15 layers). (C) Critical shear stress (τ 50) required to remove the bacteria from Cu-SURMOF 2 surfaces for different controls. Error bars indicate the standard error of six experiments in the case of Cu SURMOF 2 (10 layers) and HDT SAM, and four experiments for all other surfaces.